{"product_id":"evaluation-of-the-effect-of-welding-procedure-on-the-mechanical-properties-of-fcaw-s-and-smaw-weld-metal-used-in-the-construction-of-seismic-moment-frames","title":"Evaluation of the Effect of Welding Procedure on the Mechanical Properties of FCAW-S and SMAW Weld Metal used in the Construction of Seismic Moment Frames","description":"\u003cp\u003eThe SAC\/BD-00\/12, \u003cem\u003eEvaluation of the Effect of Welding Procedure on the Mechanical Properties of FCAW-S and SMAW Weld Metal used in the Construction of Seismic Moment Frames\u003c\/em\u003e, was funded by the Federal Emergency Management Agency (FEMA) and the California Office of Emergency Services (OES) and produced by the SAC Joint Venture (published 2000, 124 pages).\u003c\/p\u003e\u003cp\u003eThis report is printed on-demand, so a 1-3 day delay for printing may occur.\u003c\/p\u003e\u003cdiv\u003e\u003cstrong\u003e\u003cspan\u003eClick \u003ca href=\"https:\/\/cdn.shopify.com\/s\/files\/1\/0839\/4224\/4564\/files\/SAC_BD-00_12.pdf?v=1783550681\" target=\"_blank\"\u003ehere\u003c\/a\u003e to view the Title Page, Preface, and Contents.\u003c\/span\u003e\u003c\/strong\u003e\u003c\/div\u003e","brand":"Applied Technology Council","offers":[{"title":"Default Title","offer_id":48162046214356,"sku":"SAC\/BD-00\/12","price":40.0,"currency_code":"USD","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0839\/4224\/4564\/files\/SAC-BD-00-12.jpg?v=1782184461","url":"https:\/\/store.atcouncil.org\/products\/evaluation-of-the-effect-of-welding-procedure-on-the-mechanical-properties-of-fcaw-s-and-smaw-weld-metal-used-in-the-construction-of-seismic-moment-frames","provider":"The ATC Store","version":"1.0","type":"link"}